Table 1 Incinerated Thermoplastic Colloidal Characteristics - DLS

From: Carbon nanotube filler enhances incinerated thermoplastics-induced cytotoxicity and metabolic disruption in vitro

Particle

Medium

d(H, Z-avg)

(nm)

PDI

ζ (mV)

pH

σ (mS/cm)

PC

dH2O

867

0.200

−29.8

6.13

0.012

AEGM

1208

0.140

−9.73

7.41

12.3

SAGM

801

0.372

−12.7

7.48

12.2

PC-CNT

dH2O

541

0.048

−35.5

6.31

0.010

AEGM

701

0.175

−9.85

7.42

12.2

SAGM

587

0.206

−12.3

7.48

11.4

PU

dH2O

836

0.209

−6.97

5.34

0.014

AEGM

724

0.284

−10.3

7.48

12.1

SAGM

579

0.371

−10.7

7.50

11.6

PU-CNT

dH2O

603

0.233

−7.47

5.31

0.015

AEGM

559

0.375

−9.21

7.53

12.1

SAGM

417

0.305

−11

7.52

11.4

  1. Incinerated thermoplastics were diluted to 0.1 mg/mL in respective medium and assessed for intensity-based hydrodynamic diameter [d(H, Z-avg)], polydispersity index (PDI), zeta potential (ζ), suspension pH, and suspension conductivity (σ)