Skip to main content

Table 4 Summary of cellular responses to Ag ENMs with different surface charge and chemical composition

From: Impact of nanosilver on various DNA lesions and HPRT gene mutations – effects of charge and surface coating

Surface charge:

Negative

Neutral

Positive

Surface chemical composition:

Citrate

SDS

Disperbyk

Tween

Chitosan

Byk

Intercellular localisation

Cytoplasm

24 h

+

+

+

+

+

+

Nucleus

24 h

-

-

-

-

+

+

Mitochondria

24 h

-

-

-

-

+

-

Cytotoxicity

Cells morphology

2 h

-

-

-

-

+ (s)

+

24 h

+

+

-

-

+ (s)

+

Trypan blue exclusion

2 h

-

-

-

-

+

++

24 h

-

-

-

-

++

++

Relative Growth Activity

24 h

++

++

-

++

+++

+++

Genotoxicity and mutagenicity

Comet assay – Strand breaks

2 h

+

   

++

++

24 h

++

+

++

+

(x)

(x)

Comet assay – Oxidative DNA lesions

2 h

+++

+++

+++

+++

+++

+++

24 h

+++

++

++

+++

(x)

(x)

HPRT gene mutation

24 h

++ (s)

+

+

++ (s)

+

++

  1. The relative tendency of each Ag ENMs to induce cellular responses related to uptake, viability, cytotoxicity, genotoxicity and mutagenicity after 2–24 h exposure
  2. (−) no harmful effects were observed in any of tested concentrations
  3. (+) indicates a significant increase in the intracellular event in one from three-five tested concentrations/localisation in selected cells compartments/change in cells morphology
  4. (++) indicates a significant increase in the intracellular event in two-three from three-five tested concentrations
  5. (+++) a significant increase in the intracellular event in one from four-five tested concentrations
  6. (s)- Toxic effect of Ag ENMs stabilizers
  7. (x)- Fully biological effect could not be evaluated due to strong method saturation